JY · A102 Titanium kalsium tipe palapis Cr19Ni10 éléktroda stainless steel
Tujuan:Dipaké pikeun las struktur stainless steel tahan korosi, kayaning 06Cr19Ni10 na 06Cr18Ni¹1Ti jeung suhu gawé maranéhanana kudu handap 300 ℃



Item tés | C | Mn | Si | S | P | Cr | Ni | Mo | Cu |
Nilai Jaminan | ≤0.08 | 0,50~2,50 | ≤1.00 | ≤0,030 | ≤0,040 | 18.0~21.0 | 9.0~11.0 | ≤0.75 | ≤0.75 |
Hasil Umum | 0.041 | 1.35 | 0.69 | 0.008 | 0,022 | 19.5 | 9.6 | 0,064 | 0.1 |
Item tés | Rm (MPa) | A(%) |
Nilai Jaminan | ≥550 | 30 |
Hasil Umum | 600 | 42 |
Diaméterna (mm) | φ2.0 | φ2.5 | φ3.2 | Φ4.0 | φ5.0 |
Ampere (A) | 40~80 | 50~100 | 70~130 | 100~160 | 140~200 |
Catetan: 1. éléktroda kudu preheated dina suhu 300 ° C pikeun 1 hour.Pheat rod iraha wae eta dipaké.
2.Preferred catu daya DC,arus listrik teu kudu luhur.